Analisis Karakteristik Tegangan Tembus Isolasi Minyak Transformator Menggunakan Oli Sepeda Motor Shell Advance 20w-50 Dan Pertamina Mesran 20w-50

Authors

  • Adi Purwanto Umar Universitas Negeri Gorontalo
  • Sutiyono Hulopi Universitas Negeri Gorontalo
  • Lanto Mohamad Kamil Amali Universitas Negeri Gorontalo

DOI:

https://doi.org/10.55606/isaintek.v6i1.79

Keywords:

Analisis, Breakdown Voltage, Oil, Test, Transformer

Abstract

Electrical systems use high-voltage insulation as a cooling agent. A breakdown voltage will show up to indicate insulation failure if the applied voltage is greater than the liquid insulation's dielectric strength. According to SPLN '50-1982 and IEC No. 56 of 1991, the typical breakdown voltage of PERTAMINA MESRAN transformer oil insulation at 30°C temperature before cleaning or treatment is 14.59 kV / 2.5 mm. Insulation of transformer oil is categorized as a sub-interest. (in a 30 Kv/2.5 mm manner). According to SPLN '50- 1982 and IEC No. 56 of 1991, the average breakdown voltage of PERTAMINA MESRAN transformer oil insulation at 300C temperature after cleaning/remediation process is 15.18kV / 2.5mm. Insulation of transformer oil is designated as standard ((standard). usually 2.5 mm/30 Kv). According to SPLN '50- 1982 and IEC No. 56 of 1991, the average breakdown voltage of SHE LL increase the oil-insulated transformer at 30°C temperature before cleaning / treatment Process is 16.52kV / 2.5mm. Transformer oil insulation (30Kv/2.5mm nominal) is viewed as being insufficient. According to SPLN'50-1982 and IEC No. 56 of 1991, the average breakdown voltage of SHELL formed transformer oil insulation at 30°C temperature after cleaning and treatment is 22.83 kV / 2.5 mm. A division below the standard (30 Kv / 2.5 mm is common) is transformer oil insulation.

References

Marsudi, Djiteng. 2011. Pembangkitan Energi Listrik. Jakarta: Erlangga.

Arismunandar, A. 1983. Teknika Tegangana Tinggia Suplemen. Jakarta: Ghaliaa Indonesia.

Suherman,,Andri.,2016. Pengaruh, Kontaminan Air Terhadap Tegangan Tembus MinyakaTransformator Dan Minyaka Kelapa Murni. Gravity, 2 (2) 99-111.

Tobing,L.2012. Dasar-dasar Teknik Pengujian Tegangan Tinggi. Jakarta: Erlangga.

Muhaimin. 1999. Bahan-Bahan Listrik. Jakarta: Pradnya Paramita.

Abduh, Syamsir.2003. Teoria Kegagalena Isolasi. Jakarta: Universitas Trisakti.

Naidu,M.S., dan V Kamaraju.a1996. High Voltage Engineering Second Edition. aUnited States: TheaMcGraw Hill.

ASTM D1500-12, Color of Petroleum Products (ASTM Color Scale)- Test Methods, 1997.

IEC 60156, Insulating liquidsDetermination Ofa Breakdown Voltage At PoweraFrequency- Test Methods, 1995.

Saprianto.2017. Analisisa Pengaruha Pembebanan Terhadap Kekuatan Dielektrika.Minyak Isolasia Transformator 6,6 kV/380 V di PT. Inti benua Perkasatama Dumai. Jom FTEKNIK, 4 (2) 1-8.

Hidayat.Ahmad Y.2013. Analisisa Pengaruha KenaikanaTemperatur TerhadapaTeganganaTembus Dan Nilai Harapan HidupaIsolasi Padat Dan Cairan Transformator. Skripsi. TE. Fakultas Teknik. Universitas Indonesia.

Putra.I.G. N Segara. 2015. Ana Experience ina Oil Testing of Medium Voltagea Transformers. IEEE ICPADM, 1007-1010.

Wahyu Purwo Raharjo, Pemanfaatan Oli Bekas dengan Pencampuran Minyak Tanah Sebagai Atomizing Burner,Teknik Mesin, Universitas Sebelas Maret.

IEC-156, Insulating Liquid Determination of Breakdown Voltage at Power Frequency Tes Method, 1995.

Rahayu, Kholinda and Irnanda , Priyadi and Yenni , Suhartini, Analisis Karakteristik Dielektrik Minyak Jagung Sebagai Alternatif Bahan Isolasi Cair. Undergraduated thesis, Fakultas Teknik Universitas Bengkulu.

Downloads

Published

2023-05-09

How to Cite

Adi Purwanto Umar, Sutiyono Hulopi, & Lanto Mohamad Kamil Amali. (2023). Analisis Karakteristik Tegangan Tembus Isolasi Minyak Transformator Menggunakan Oli Sepeda Motor Shell Advance 20w-50 Dan Pertamina Mesran 20w-50. Jurnal Informasi, Sains Dan Teknologi, 6(1), 09–18. https://doi.org/10.55606/isaintek.v6i1.79